High-speed hair grafting machine correct process flow
Zostaw wiadomość
1, The fair use of hair (pile) slurry in the wool planting process plays a crucial role, first in the application of hair (pile) slurry first participate in the necessary quantitative additives (1.5%-2%) or additives add 1 to 1 water mixing mixing, and then add the pulp mixing and average, the modulated pulp needs to be used immediately, can not be placed for too long (within 8 hours), otherwise cross-linking will occur at the deformation temperature and affect the use, which is a matter to be paid attention to in the operation. If the wool slurry is too thick in printing, you can add an appropriate amount of water to dilute it, which helps to operate benignly.
2. It is recommended to use 800 mesh (80 mesh) plates, screen printing: pay attention to the moment of the final printing of the wool (pile) paste and the hair planting operation, must not be 1 minute apart, the number of printing is adjusted according to the relevant fabric, time and other factors.
3. The cloth is naturally dry, and it can be washed at 60 °C after 24 hours. If the quality is strictly required by the customer, it is necessary to bake, 160 °C, 10-60 seconds, of course, the baking temperature, Shaoguang also needs to be adjusted according to the coherent fabric, pleading, etc.
4. The final process of cloth wool planting liquidates the tail process, and after using the hair suction machine to suck the hair, the remaining part of the wool products of the cloth is glued with adhesive paper.